Victor,
Ni-B is also electroless
Vladimir
Sent from my BlackBerry 10 smartphone on the Rogers network.
Original Message
From: Victor Hernandez
Sent: Monday, January 26, 2015 07:49
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: [TN] Nickel Question
Fellow TechNetters:
Does Ni boron (electroplated process) and Ni Phosphorous (ENIG process) have the same hardness?