Hi Vicyor,
For hard gold ad far as I know it's Ni (electroplated), while for ENIG it's Ni-P (rarely Ni-B) and it's electroless.
Regards,
Vladimir
Sent from my BlackBerry 10 smartphone on the Rogers network.
Original Message
From: Victor Hernandez
Sent: Friday, January 23, 2015 12:54
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: [TN] Chemistry Question for GURUs
Fellow TechNetters:
Are the nickel properties for a hard gold plating process similar to an ENIG plating process.
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________