TECHNET Archives

January 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Date:
Mon, 26 Jan 2015 16:14:31 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, David Hillman <[log in to unmask]>
Subject:
From:
David Hillman <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (116 lines)
Or I was typing too fast. Let's try this again:

 I don't have the hardness values for NiB but for NiP, the hardness for a
deposit in
the 7-9% range is 550-600 kp/mm2.

On Mon, Jan 26, 2015 at 3:41 PM, Wayne Thayer <[log in to unmask]> wrote:

> Classical but-for swap going on there....
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of David Hillman
> Sent: Monday, January 26, 2015 4:38 PM
> To: [log in to unmask]
> Subject: Re: [TN] Nickel Question
>
> Hi Victor - I don't have the NiB for for NiP, the hardness for a deposit in
> the 7-9% range is 550-600 kp/mm2.
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
>
> On Mon, Jan 26, 2015 at 3:23 PM, Victor Hernandez <
> [log in to unmask]> wrote:
>
> > Back to the original question about nickel hardness between Ni B and Ni
> P.
> >
> > Victor,
> >
> > -----Original Message-----
> > From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
> > Sent: Monday, January 26, 2015 2:02 PM
> > To: [log in to unmask]
> > Subject: Re: [TN] Nickel Question
> >
> > Usually, but not always. Oftentimes a tungsten/nickel/boron finish is
> > electroplated instead of the more common chromium, and when
> > electroplated it is much harder than the electroless plating (it is
> > generally thicker).
> > But this is usually done for mechanical components.
> >
> > http://www.osti.gov/scitech/biblio/72974-QMzJhC/webviewable/
> > http://asterionstc.com/tungsten-nickel-boron-electroplating-system/
> >
> > But I have never heard of electroplated TNB being used as a circuit
> > board finish. I don't think you can solder to it, if that is what you are
> > asking.
> >
> > -----Original Message-----
> > From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev
> > Sent: Monday, January 26, 2015 6:53 AM
> > To: [log in to unmask]
> > Subject: Re: [TN] Nickel Question
> >
> > Victor,
> >
> > Ni-B is also electroless
> >
> > Vladimir
> >
> > Sent from my BlackBerry 10 smartphone on the Rogers network.
> >   Original Message
> > From: Victor Hernandez
> > Sent: Monday, January 26, 2015 07:49
> > To: [log in to unmask]
> > Reply To: TechNet E-Mail Forum
> > Subject: [TN] Nickel Question
> >
> > Fellow TechNetters:
> >
> > Does Ni boron (electroplated process) and Ni Phosphorous (ENIG
> > process) have the same hardness?
> >
> > Victor,
> >
> >
> > ______________________________________________________________________
> > This email has been scanned by the Symantec Email Security.cloud service.
> > For more information please contact helpdesk at x2960 or
> > [log in to unmask]
> > ______________________________________________________________________
> >
> > ______________________________________________________________________
> > This email has been scanned by the Symantec Email Security.cloud service.
> > For more information please contact helpdesk at x2960 or
> > [log in to unmask]
> > ______________________________________________________________________
> >
> > ______________________________________________________________________
> > This email has been scanned by the Symantec Email Security.cloud service.
> > For more information please contact helpdesk at x2960 or
> > [log in to unmask]
> > ______________________________________________________________________
> >
> > ______________________________________________________________________
> > This email has been scanned by the Symantec Email Security.cloud service.
> > For more information please contact helpdesk at x2960 or
> > [log in to unmask]
> > ______________________________________________________________________
> >
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2