Can't argue about the manual handling but from experience there isn't anything left on our boards as when it's pulled off when warm it comes off in one piece.
To be fair we are only low volume but high cost so works for us.
-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]]
Sent: 09 December 2014 17:56
To: Braddock, Iain (UK); TechNet E-Mail Forum
Subject: RE: [TN] BGA Reflow Issue
*** WARNING ***
This mail has originated outside your organization, either from an external partner or the Global Internet.
Keep this in mind if you answer this message.
Yes, but usually it is not peeled off 100% and a lot ends up in the wash filters.
It also adds a lot of manual handling and more labor hours.
-----Original Message-----
From: Braddock, Iain (UK) [mailto:[log in to unmask]]
Sent: Tuesday, December 09, 2014 11:20 AM
To: Stadem, Richard D.; TechNet E-Mail Forum
Subject: RE: [TN] BGA Reflow Issue
Dean,
The 'P' variant is not expected to be washed off as it's peelable.
-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]]
Sent: 09 December 2014 14:59
To: TechNet E-Mail Forum; Braddock, Iain (UK)
Subject: RE: [TN] BGA Reflow Issue
*** WARNING ***
This mail has originated outside your organization, either from an external partner or the Global Internet.
Keep this in mind if you answer this message.
The problem with peelable maskants is that they do not disappear in the wash, they will clog the filters and present FOD on the workbench surfaces, rub off, etc.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Braddock, Iain (UK)
Sent: Tuesday, December 09, 2014 8:53 AM
To: [log in to unmask]
Subject: Re: [TN] BGA Reflow Issue
Dave,
I agree with Steve, we use Wondermask but the 'P' variant which is peelable; comes off very easily when warm leaving no residue.
We use it for BGAs as large 50mm square, running a line down two opposing sides works a treat.
Regards,
Iain
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: 09 December 2014 14:23
To: [log in to unmask]
Subject: Re: [TN] BGA Reflow Issue
*** WARNING ***
This mail has originated outside your organization, either from an external partner or the Global Internet.
Keep this in mind if you answer this message.
Hi Dave,
What about Techspray WSOL mask? I have used it for big heavy SMT power inductors when they've been on both sides of the board because they've fallen off once in a while during the second reflow. Haven't used it on BGA's though...
Steve
On Tue, Dec 9, 2014 at 6:42 AM, David Hillman < [log in to unmask]> wrote:
> Hi gang - looking for an adhesive suggestion. I have an assembly in
> which a heavy BGA was accidently located on process side one (bottom)
> so that when we reflow process side two (top) the BGA is doing its best to fall off.
> Unfortunately I can't reverse my process order for a couple of reasons
> so I am looking for a temporary fix until I can get the assembly
> revised. I was thinking of using some type of adhesive to temporarily
> hold the BGA in place during reflow - tack down the corners sort of
> action. Does anyone have any adhesive (ideally temporary, water
> washable/removable) suggestions I can investigate?
>
> TIA
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
********************************************************************
This email and any attachments are confidential to the intended recipient and may also be privileged. If you are not the intended recipient please delete it from your system and notify the sender. You should not copy it or use it for any purpose nor disclose or distribute its contents to any other person.
MBDA UK Limited, a company registered in England and Wales, registration number 3144919 whose registered office is at Six Hills Way, Stevenage, Hertfordshire, SG1 2DA, England.
********************************************************************
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
********************************************************************
This email and any attachments are confidential to the intended recipient and may also be privileged. If you are not the intended recipient please delete it from your system and notify the sender. You should not copy it or use it for any purpose nor disclose or distribute its contents to any other person.
MBDA UK Limited, a company registered in England and Wales, registration number 3144919 whose registered office is at Six Hills Way, Stevenage, Hertfordshire, SG1 2DA, England.
********************************************************************
********************************************************************
This email and any attachments are confidential to the intended recipient and may also be privileged. If you are not the intended recipient please delete it from your system and notify the sender. You should not copy it or use it for any purpose nor disclose or distribute its contents to any other person.
MBDA UK Limited, a company registered in England and Wales, registration number 3144919 whose registered office is at Six Hills Way, Stevenage, Hertfordshire, SG1 2DA, England.
********************************************************************
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|