Good afternoon all,
I am wondering if anyone in the Net knows of any studies on dielectric
strength of conformal coating type and/or thickness, vs. altitude? Along
the lines of protection against arcing and corona (effect, not the beer).
I figured if anyone knows, this group would.
Doug Pauls
Principal Materials and Process Engineer
Rockwell Collins