Guy,
When I first read your post very early this morning, my eyes were blurry
yet. I thought the Title was "ENIG causes drinking?"
Possibly that is still applicable??
Steve C
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
Sent: Friday, December 12, 2014 8:19 AM
To: [log in to unmask]
Subject: [TN] ENIG causes shrinking?
One of our suppliers sent us a batch of boards that have a feature
registration shift. The laminate is Rodgers RO4003. Has anyone ever heard
of the ENIG process causing this kind of shrinkage?
" We measured all the panels after etching on the X-ray
machine for scale and shift using 4 etched targets on four corners of the
panel. After these 4 targets are measured top and bottom simultaneously,
program calculates shrink, stretch and top to bottom registration.
For the last batch of panels processed we tried dialing in
the scale factors on LDI to get the pad features to nominal. we couldn't get
it to nominal but were slightly short about .3 mils per inch in both X and Y
from nominal. By doing the math it was determined it will still be within
spec. All these measurements were done after etch before ENIG finish.
After the panels came back we didn't measure them, went
straight to rout and shipped to RDIS.
Since the boards are still failing for TPD after all these
precautions, Only other variable is the material shrinkage after ENIG
process.
We had few panels of part numbers that were not laser cut
yet after ENIG. All these panels were measured after etch before sending it
out to ENIG and they were slightly long about .3 mil per inch. I then
measured the same panels (after ENIG) today late evening and they were
right at nominal which means they shrunk by about .3 mil per inch during
ENIG process.
The batch of boards that you have failing for TPD tolerance,
were short by about .3 mil per inch before going to ENIG and shrunk
additional .3 mil per inch after ENIG. They were about .6 mil per inch
shorter than nominal. The board length at about 5 inches in the long
dimension makes it about 3 mil short in long axis and .5 mil in short axis
there by failing the TPD tolerances."
Guy Ramsey | R&D Interconnect Solutions | Process Manager | [log in to unmask]
| Mobile: 610-349-2519 | Office: 610-443-2299 |
1660 East Race Street | Allentown, PA 18109 USA | www.rdis.com
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|