Hi gang - looking for an adhesive suggestion. I have an assembly in which a
heavy BGA was accidently located on process side one (bottom) so that when
we reflow process side two (top) the BGA is doing its best to fall off.
Unfortunately I can't reverse my process order for a couple of reasons so I
am looking for a temporary fix until I can get the assembly revised. I was
thinking of using some type of adhesive to temporarily hold the BGA in
place during reflow - tack down the corners sort of action. Does anyone
have any adhesive (ideally temporary, water washable/removable) suggestions
I can investigate?