TECHNET Archives

November 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Datacom - Juliano Ribeiro <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Datacom - Juliano Ribeiro <[log in to unmask]>
Date:
Thu, 20 Nov 2014 09:46:14 -0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (66 lines)
Hi to all,

 

We are analyzing my wave solder pot (contamination level).

But we found in the IPC different limits. 

IPC-006B <>IPC-001C

 

                IPC06     IPC01

Ag           0,1          0,1

Al            0,005     0,006

As           0,03        0,03

Au          0,05        0,03

Bi            0,1          0,25

Cd           0,002     0,005

Cu           0,08        0,3

Fe           0,02        0,02

Ni            0,01        0,01

Zn           0,003     0,005

 

In this case what is the correct to analyze my solder pot?

 

Ps.: Alloy 63/37

_____________________________

Juliano Bettim Ribeiro

DATACOM 

ENGENHARIA DE PROCESSOS 
Rua América Nº 1000 - Eldorado do Sul - RS CEP: 92990-000 
+55 (51) 8446-2135

+55 (51) 3933-3000 

Ramal: 3484
 <mailto:[log in to unmask]> [log in to unmask] 
 <http://www.datacom.ind.br/> www.datacom.ind.br

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2