Hi to all,
We are analyzing my wave solder pot (contamination level).
But we found in the IPC different limits.
IPC-006B <>IPC-001C
IPC06 IPC01
Ag 0,1 0,1
Al 0,005 0,006
As 0,03 0,03
Au 0,05 0,03
Bi 0,1 0,25
Cd 0,002 0,005
Cu 0,08 0,3
Fe 0,02 0,02
Ni 0,01 0,01
Zn 0,003 0,005
In this case what is the correct to analyze my solder pot?
Ps.: Alloy 63/37