TECHNET Archives

October 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Craig Sullivan <[log in to unmask]>
Date:
Wed, 15 Oct 2014 14:52:41 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M. [Contractor]" <[log in to unmask]>
Message-ID:
Subject:
From:
"Wenger, George M. [Contractor]" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (72 lines)
If you try to hide the marking by covering it up with marking ink, paint, epoxy, etc. you could still have a problem with someone who was trying to reverse engineer the product because we've taken components that were cover up and very carefully cross sectioned though the coating and stopped when we got very close to the marking and while it was very difficult and not easy to read we were able to determine what the marking said.  The best way we know is to mechanically grind away the marking and then cover the top of the component with marking ink, paint, epoxy, etc.

Regards,
George
George M. Wenger
Failure Signature & Characterization Lab LLC
609 Cokesbury Road, High Bridge, NJ 08829
(908) 638-8771 Home  (732) 309-8964 Mobile
E-mail [log in to unmask]
[log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Craig Sullivan
Sent: Wednesday, October 15, 2014 3:03 PM
To: [log in to unmask]
Subject: [TN] Obscure IC part markings

I have a customer requirement to "apply an electronics grade epoxy over component x that will obscure part the part marking." They are trying to prevent reverse engineering of their product. There are of course a multitude of epoxies, but dispensing onto small ICs, etc., can be a challenge. 

 

I know about micro abrasion processes and such but I'm curious how others would handle this requirement?

 

Craig Sullivan

Manufacturing Engineer / IT Administrator

Phone:  +1.607.266.0480 x115

Fax:  +1.607.266.0482

Email:  <mailto:[log in to unmask]> [log in to unmask]

Web:   <http://www.mplinc.com/> www.mplinc.com

 

MPL, Inc.

41 Dutch Mill Road  |  Ithaca  |  NY  |  14850

P Please consider the environment before printing this e-mail.

 

  _____  

Confidentiality Notice:
This e-mail contains privileged and confidential information which is the property of MPL Incorporated, intended only for the use of the intended recipient(s). Unauthorized use or disclosure of this information is prohibited. If you are not an intended recipient, please immediately notify MPL Incorporated and destroy any copies of this email. Receipt of this e-mail shall not be deemed a waiver by MPL Incorporated of any privilege or the confidential nature of the information.

Export Control:
This message is intended only for the addressee and may contain information that is company confidential or privileged. Any technical data in this message may be exported only in accordance with the U.S. International Traffic in Arms Regulations (22 CFR Parts 120-130) or the Export Administration Regulations (15 CFR Parts 730-774). Unauthorized use is strictly prohibited and may be unlawful. If you are not the intended recipient, or the person responsible for delivering to the intended recipient, you should not read, copy, disclose or otherwise use this message. If you have received this email in error, please delete it, and advise the sender immediately.

 

 

 



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2