Graham,
I seem to remember Kester had a swab test kit to use in checking for
lead, not sure if it will work large scale but it might be worth a look.
pat goodyear
retired CT
On Tue, Sep 16, 2014 at 11:37 AM, Graham Collins wrote:
> Good day TechNet
> We are a late arrival to the lead-free party, as our customers thus
> far are exempt. But a couple of them see the writing on the wall and
> are moving toward RoHS compliance. Which leads me to two questions
> with regards to our testing of parts to ensure compliance.
>
> The first question - what XRF? We are concerned with price given that
> we are dipping our feet here, does anyone have a recommendation for a
> good but inexpensive unit?
>
> Second question is concerning alternative test methods, a customer is
> planning to use 3M LeadCheck swabs (LC-8S10C) to ensure no lead.
> Given that the product is described as for use on painted surfaces I
> don't think this is intended as a way to verify lead-free status on
> electronics. Any comments on this?
>
> Thanks!
>
> --
> regards,
>
> Graham Collins
> Senior Process Engineer
> Sunsel Systems
> (902) 444-7867 ext 211
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
> service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|