TECHNET Archives

September 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Syed Ahmad <[log in to unmask]>
Date:
Mon, 15 Sep 2014 16:47:21 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Yuan-chia Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Yuan-chia Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"; delsp=yes; format=flowed
MIME-Version:
1.0 (Apple Message framework v753.1)
Parts/Attachments:
text/plain (23 lines)
you mean Al shield tape with adhesive?  commonly used, but not for  
harsh environment.  you didn't mention designed life time either...
my 2 cents.
        jk
On Sep 15, 2014, at 4:22 PM, Syed Ahmad wrote:

> Looking for observations on an aluminum plate mechanically attached  
> to a gold plated PCB for shielding purposes: Galvanic reactions?  
> Corrosion possibilities?
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud  
> service.
> For more information please contact helpdesk at x2960 or  
> [log in to unmask]
> ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2