TECHNET Archives

September 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 30 Sep 2014 16:13:31 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Juan T. Marugán" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Type:
text/plain; charset="utf-8"
Content-Transfer-Encoding:
quoted-printable
From:
"Juan T. Marugán" <[log in to unmask]>
Parts/Attachments:
text/plain (8 lines)
Hello.

We have to send some BGAs components to a specialized company to change the balls from LF to tin lead, and we are thinking in how to validate this process. My question is if there is a method or a standard (IPC?) to do this task. Is it necessary or can we trust in the know-how of the supplier?

Thank you so much for your expert comments.