Yes it's hard to work with it but it doesn't susceptible to Au embrittlement to the same degree :-).
Regards,
Vladimir
Sent from my BlackBerry 10 smartphone on the Rogers network.
Original Message
From: Guy Ramsey
Sent: Friday, September 19, 2014 10:04 AM
To: 'TechNet E-Mail Forum'; [log in to unmask]
Reply To: [log in to unmask]
Subject: RE: [TN] Au embrittlement
Yes, it is the tin.
I recently discussed this with engineers at Indium Corporation.
They recommended indium-silver solder. It was hard to work with.
Guy
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev
Sent: Friday, September 19, 2014 9:17 AM
To: [log in to unmask]
Subject: [TN] Au embrittlement
I'm trying to find information on whether Sn-Bi based solders are susceptible to Au embrittlement in a similar way as Sn and Sn-Pb-based solders do.
I don't see why they wouldn't but need some confirmation.
As always, thank you very much in advance for constructive answers.
Regards,
Vladimir
Sent from my BlackBerry 10 smartphone on the Rogers network.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|