TECHNET Archives

August 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan TEMPEA <[log in to unmask]>
Date:
Thu, 28 Aug 2014 10:32:10 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Douglas Pauls <[log in to unmask]>
Subject:
From:
Douglas Pauls <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (74 lines)
Ioan,
I would suggest you start with March Plasma Systems, a division of Nordson.
 They have a wealth of information on plasma processing and are pretty good
about sharing information.

http://www.nordson.com/en-us/divisions/march/pages/default.aspx

If you are looking for something more along the lines of a textbook, you
can consider:
Handbook of Plasma Processing Technology, by Rossnagel, Cuomo and Westwood.
 Noyes Publications
That handbook was originally published in 1990, so I am not sure how
current it is.  I have a copy and it is OK.

I would start with March.  They probably have the most up to date
information on the science.

The people out at Plasma Ruggedized Systems in Huntington Beach, CA are
also very good at plasma processing and can answer more process related
questions.


Doug Pauls
Principal Materials and Process Engineer
Rockwell Collins


On Thu, Aug 28, 2014 at 10:17 AM, Ioan TEMPEA <
[log in to unmask]> wrote:

> Dear Technos,
>
> Talking about the surface energy as a property of a surface that will get
> conformal coated, for instance, (as opposed to the surface tension which
> belongs to the coating material).
>
> From what I've read vacuum bakeout will reduce this surface energy and
> plasma cleaning will increase it. Where can I get academia on the physics
> of the surface energy (where it comes from, why plasma cleaning and vacuum
> bakeout affect it, etc.)?
>
> Thanks,
>
> Ioan Tempea, P. Eng.
> Manufacturing Engineer
> Satellite Systems
> MDA
> 21025 TransCanada Highway
> Ste-Anne-de-Bellevue, Qc, Canada H9X 3R2
> Tel: +1-514-457-2150-3556
> www.mdacorporation.com<http://www.mdacorporation.com>
>
> This e-mail, and any attachments, are intended solely for the use of the
> intended recipient(s) and may contain legally privileged, proprietary
> and/or confidential information. Any use, disclosure, dissemination,
> distribution or copying of this e-mail and any attachments for any purposes
> that have not been specifically authorized by the sender is strictly
> prohibited. If you are not the intended recipient, please immediately
> notify the sender by reply e-mail and permanently delete all copies and
> attachments.
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2