TECHNET Archives

July 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Wayne Thayer <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Date:
Tue, 8 Jul 2014 20:50:47 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (52 lines)
Hi Peter-

SAC305 is well known for eroding metals. 325C sounds pretty darned hot to
me! Why so high?

I have run a solder fountain rework station filled with SAC305, and it was
very difficult to stop it from eroding the ends of the via barrels. That was
only at 230C!

Wayne Thayer

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Wong
Sent: Tuesday, July 08, 2014 4:32 PM
To: [log in to unmask]
Subject: [TN] Dissolving pins

Hi Everyone,

We ran some assemblies where after selective soldering with SAC305, the
phosphor bronze leads on a Harwin connector look to have been dissolved.
The solder pot temperature is set at 325 deg C and we dwelled on each pin
for no more than 3 seconds.  We are using an OA flux.  Harwin tells me that
the melting point of the pins is 954 deg C.

We are having the solder in our selective solder pot analyzed to see if
there is anything out of spec that could be causing this.

Has anyone else experienced something similar or does anyone have an idea as
to what could be causing this?

A photo is available at the following link.
http://ipc-technet.groupsite.com/galleries/show/27385

Thanks
Peter


________________________________
The enclosed documents are proprietary items to Silicon Forest Electronics'
(SFE) customers. They shall not be reproduced nor disclosed for any purpose
except as specified in writing from an authorized agent of SFE. These
documents may contain data restricted for export by the International
Traffic in Arms Regulations (ITAR) section of the Arms Export Control Act
(or the Export Administration Act). Violators are subject to severe criminal
penalties.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

ATOM RSS1 RSS2