Bev Christian <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Thu, 31 Jul 2014 15:57:26 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (38 lines)
Paul,
Do NOT use a silicone.
Bev

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Jackson
Sent: Wednesday, July 30, 2014 12:48 PM
To: [log in to unmask]
Subject: [TN] Conformal coating for Sulfur environments

We have a customer whose PCBAs are subjected to flower of sulfur rich 
environments. The sulfur quickly corrodes any area not covered in 
soldermask. They would like to use a conformal coating but their 
research to-date has only come up with one solution which has published 
data specifically concerning sulfur and the coating is too viscous for 
their application.

Does anyone have experience with a conformal coating which is proven to 
survive in an environment with sulfur?

Any help would be greatly appreciated.

Thanks,

Paul
Omni Circuit Boards

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 