All the more reason to identify what the material is (i.e., solder or fill material?)
Regards,
George
George M. Wenger
Failure Signature & Characterization Lab LLC
609 Cokesbury Road, High Bridge, NJ 08829
(908) 638-8771 Home (732) 309-8964 Mobile
E-mail [log in to unmask]
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Hillman
Sent: Tuesday, July 29, 2014 3:21 PM
To: [log in to unmask]
Subject: Re: [TN] Trying to figure out possible mechanism for contamination
Hi gang - I had the same first impression as Dick that these were solder splatters from reflow/wave/stencil but when I looked closer, it the splatters are very very uniform in size plus the center "dot' is equally uniform. Someone had mention a filled micro via delamin-ish problem could be the root cause. Take a look at the photo again - doesn't it seem that these are too uniform for a solder splatter root cause?
Dave Hillman
Rockwell Collins
[log in to unmask]
On Tue, Jul 29, 2014 at 11:30 AM, Richard Krug <[log in to unmask]> wrote:
> To me it looks like solder paste spatter / fines that landed on ENIG
> surface. Can be caused by too steep a ramp rate during preheat stage
> of reflow profile. Was measured reflow profile within manufacturer's spec?
>
> Dick Krug, CSSBB, CSMTPE
> Lead Process Engineer
> Sparton Brooksville, LLC
> 30167 Power Line Road
> Brooksville, FL 34602-8299
> p (352) 540-4012 (Internal Ext. 2012) [log in to unmask]
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of John Foster
> Sent: Tuesday, July 29, 2014 12:13 PM
> To: [log in to unmask]
> Subject: [TN] Trying to figure out possible mechanism for
> contamination
>
> We have been seeing a problem recently on several different CCA'S that
> we are having assembled.
> The boards are ENIG with plug and plate. The assembly shop is
> assuring us that these gold areas are being Protected during the
> entire assembly process with kapton tape.
> I was thinking it was flux splatter since the areas are always almost
> perfectly circular.
> The locations are very random and range from nothing to what is in the
> picture.
> Is there any other mechanism that might be causing this? On our next
> run I am going to go to the shop To witness the taping. But I was
> curious if maybe it's some other cause.
> Mr. Gregory was kind enough to post a picture.
> http://stevezeva.homestead.com/spots.jpg
>
> Any thoughts would be appreciated
> Thank You
> John Foster
> L3 Communicatons
>
> Confidentiality Notice: The information contained in this message is
> intended only for the use of the addressee, and may be confidential
> and/or privileged. If the reader of this message is not the intended
> recipient, or the employee or agent responsible to deliver it to the
> intended recipient, you are hereby notified that any dissemination,
> distribution of copying of this communication is strictly prohibited.
> if you have received this communication in error, please notify the sender immediately.
>
> Warning: This document may contain technical data within the
> definition of the International Traffic in Arms Regulation (ITAR) and
> is subject to the export control laws of the U.S. Government.
> Transfer of this data by any means to a foreign person, whether in the
> United States or abroad, without an export license or other approval
> from the U.S. Department of State, is strictly prohibited
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|