Hello Peter - well, something is wrong as 3 seconds of dwell in a SAC305
selective solder should not produce that result. How confident that the 3
second value is correct?
Dave Hillman
Rockwell Collins
[log in to unmask]
On Tue, Jul 8, 2014 at 3:32 PM, Peter Wong <[log in to unmask]> wrote:
> Hi Everyone,
>
> We ran some assemblies where after selective soldering with SAC305, the
> phosphor bronze leads on a Harwin connector look to have been dissolved.
> The solder pot temperature is set at 325 deg C and we dwelled on each pin
> for no more than 3 seconds. We are using an OA flux. Harwin tells me that
> the melting point of the pins is 954 deg C.
>
> We are having the solder in our selective solder pot analyzed to see if
> there is anything out of spec that could be causing this.
>
> Has anyone else experienced something similar or does anyone have an idea
> as to what could be causing this?
>
> A photo is available at the following link.
> http://ipc-technet.groupsite.com/galleries/show/27385
>
> Thanks
> Peter
>
>
> ________________________________
> The enclosed documents are proprietary items to Silicon Forest
> Electronics' (SFE) customers. They shall not be reproduced nor disclosed
> for any purpose except as specified in writing from an authorized agent of
> SFE. These documents may contain data restricted for export by the
> International Traffic in Arms Regulations (ITAR) section of the Arms Export
> Control Act (or the Export Administration Act). Violators are subject to
> severe criminal penalties.
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|