I've had one customer who asked for protection from Sulfuric gas and we
applied Parylene. It passed their testing but I do not have the results.
There is plenty of data out there on the barrier strengths of Parylene so
it should not be hard to find. I always recommend testing though, to verify
it will work for the individual application.
Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com
On Wed, Jul 30, 2014 at 3:03 PM, McGlaughlin, Jeffrey A <
[log in to unmask]> wrote:
> Have they looked into Parylene (poly-paraxylylene) coating. The coating is
> thin mechanic lay and thermally stable and will withstand exposure to most
> chemicals including Hydrofluoric Acid.
>
>
> Jeffrey McGlaughlin, C.I.D.
> Engineering Designer
>
> Battelle
> 505 King Avenue
> Columbus Ohio 43201-2693
> [log in to unmask]
>
> This message is intended only for the use of the individual or entity to
> which it is addressed, and may contain information that is privileged,
> confidential and/or otherwise exempt from disclosure under applicable law.
> If the reader of this message is not the intended recipient or the employee
> or agent responsible for delivering the message to the intended recipient,
> any disclosure, dissemination, distribution, copying or other use of this
> communication or its substance is prohibited. If you have received this
> communication in error, please return to the sender and delete from your
> computer system.
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Jackson
> Sent: Wednesday, July 30, 2014 12:48 PM
> To: [log in to unmask]
> Subject: [TN] Conformal coating for Sulfur environments
>
> We have a customer whose PCBAs are subjected to flower of sulfur rich
> environments. The sulfur quickly corrodes any area not covered in
> soldermask. They would like to use a conformal coating but their
> research to-date has only come up with one solution which has published
> data specifically concerning sulfur and the coating is too viscous for
> their application.
>
> Does anyone have experience with a conformal coating which is proven to
> survive in an environment with sulfur?
>
> Any help would be greatly appreciated.
>
> Thanks,
>
> Paul
> Omni Circuit Boards
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|