Now that looks very much like a plating defect. Time for a SEM and
cross-section assessment.
Dave Hillman
Rockwell Collins
[log in to unmask]
On Wed, Jul 30, 2014 at 8:02 AM, Steve Gregory <[log in to unmask]> wrote:
> Morning John,
>
> I have your second photo posted, it's here:
>
> http://stevezeva.homestead.com/ring.jpg
>
> This looks interesting!
>
> Steve
>
>
> On Tue, Jul 29, 2014 at 5:56 PM, <[log in to unmask]> wrote:
>
> > Hi steve
> >
> > I managed to get to a good microscope this afternoon. Everyone of these
> > spots looks like someone circled it* w*ith a magic marker.
> >
> > Would you mind posting one more pic for me.
> >
> > Thanks
> >
> > John Foster
> >
> >
> >
>
> --
>
>
> This email and any attachments are only for use by the intended
> recipient(s) and may contain legally privileged, confidential, proprietary
> or otherwise private information. Any unauthorized use, reproduction,
> dissemination, distribution or other disclosure of the contents of this
> e-mail or its attachments is strictly prohibited. If you have received this
> email in error, please notify the sender immediately and delete the
> original.
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|