And get a different PWB supplier. The ones I work with would have offered to re-drill the holes to remove the small amounts of copper plating that were not supposed to be there in the first place, not call out some improperly applied spec that somehow could be mis-interpreted to mean the copper plating can be in holes clearly marked as unplated on the fab drawing.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Tuesday, June 10, 2014 10:38 AM
To: [log in to unmask]
Subject: Re: [TN] Plating in non-plated holes - again
Drill after ENIG
Brian
On 10.06.2014 18:26, Henry Rekers wrote:
> Hey there technetters. A while back, I sent a message about enig plating
> contamination in NON-plated holes. I've bounced it back to the board
> shop saying that it is unacceptable, but they claim it is due to 6012
> 3.5.2
> I also think it's unacceptable in the 4552 spec. The design
> documentation clearly states non-plated. It's not plated, just partially
> plated.
>
> Any advice?
>
> Thanks.
> ______________________________________________________________________
> _______________
>
>
> Henry Rekers P. Eng | Schneider Electric | Global Supply Chain |
> Senior Manufacturing Engineer
> Phone: +1-250-652-7100 ext. 7510 | Toll Free: +1-866-466-7627 ext.
> 7510 | Fax: +1-250-544-2390 |
> Email: [log in to unmask] | Site:
> www.schneider-electric.com | Address: 2195 Keating Cross Road,
> Saanichton, BC, Canada, V8M 2A5
> *** Please consider the environment before printing this e-mail
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|