Thanks Dave,
I will cross section it and see.
Regards,
Gil
-------- הודעה מקורית --------
מאת: [log in to unmask]
תאריך:02/06/2014 7:42 PM (GMT+02:00)
אל: TechNet E-Mail Forum ,Zilber Gil
נושא: Re: [TN] Capacitor - strange soldering behavior
Hi Gil - if the capacitor has no barrier plating then what you may be observing is the underlying capacitor metallization leaching into the solder joint causing changes in the solder joint microstructure. In general, the solder microstructure changes won't be the issue but the leaching causes loss of adhesion of the capacitor metallization resulting in loss/degradation of component functionality.
Dave
From: Zilber Gil <[log in to unmask]>
To: <[log in to unmask]>
Date: 06/02/2014 10:12 AM
Subject: Re: [TN] Capacitor - strange soldering behavior
Sent by: TechNet <[log in to unmask]>
________________________________
Hi Dave,
I did not cross section the capacitor, I will do it next week and update you, also will check the underlying metallization,I did not find it on the datasheet.
Thanks,
Gil
________________________________
From: David Hillman [mailto:[log in to unmask]]
Sent: Monday, June 02, 2014 5:36 PM
To: TechNet E-Mail Forum; Zilber Gil
Subject: Re: [TN] Capacitor - strange soldering behavior
Hi Gil - two questions: (1) Does the capacitor have a barrier layer of copper or nickel to prevent the underlying metallization from leaching into the solder joint?; (2) Have you completed a cross section to assess the solder joint microstructure?
Dave Hillman
Rockwell Collins
[log in to unmask]<mailto:[log in to unmask]>
On Thu, May 29, 2014 at 9:01 AM, Zilber Gil <[log in to unmask]<mailto:[log in to unmask]>> wrote:
Hello Technet,
While soldering this ceramic capacitor (http://ipc-technet.groupsite.com/gallery/27235), its looks like that the capacitor suck the solder from the PCB`s pad to the capacitor pad and the color is now grayish and porosity. XRF found Sn, Pb, Cu on the capacitor pad. PCB solderability was good and the profile was SnPb at 225 deg C under Nitrogen. Other capacitors and components on the board look normal with shine soldering.
Can anybody seen something like that before? Any ideas?
Thanks and have a wonderful weekend.
Dr. Gil Zilber
Technologist, Elta system Ltd.
The information contained in this communication is proprietary to Israel Aerospace Industries Ltd. and/or third parties, may contain confidential or privileged information, and is intended only for the use of the intended addresse thereof. If you are not the intended addressee, please be aware that any use, disclosure, distribution and/or copying of this communication is strictly prohibited. If you receive this communication in error, please notify the sender immediately and delete it from your computer.
Thank you.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
The information contained in this communication is proprietary to Israel Aerospace Industries Ltd. and/or third parties, may contain confidential or privileged information, and is intended only for the use of the intended addresse thereof. If you are not the intended addressee, please be aware that any use, disclosure, distribution and/or copying of this communication is strictly prohibited. If you receive this communication in error, please notify the sender immediately and delete it from your computer.
Thank you.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
The information contained in this communication is proprietary to Israel Aerospace Industries Ltd. and/or third parties, may contain confidential or privileged information, and is intended only for the use of the intended addresse thereof. If you are not the intended addressee, please be aware that any use, disclosure, distribution and/or copying of this communication is strictly prohibited. If you receive this communication in error, please notify the sender immediately and delete it from your computer.
Thank you.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|