There is a lot of information on tin whiskers. It very seldom occurs
with tin-lead, and more likely to be seen with lead free. Some denizens
of tech net are studying this phenomenon in detail.
thor.inemi.org/webdownload/.../SMTAI-04_tin_whiskers.pdf ?
Karen Tellefsen - Electrical Testing
Alpha / 109 Corporate Blvd./ S. Plainfield, NJ 07080
[log in to unmask]
908-791-3069
From: Datacom - Juliano Ribeiro <[log in to unmask]>
To: <[log in to unmask]>,
Date: 06/02/2014 10:05 AM
Subject: [TN] Tin Whisker
Sent by: TechNet <[log in to unmask]>
Dears,
Why occurs the Tin Whisker? Is it possible tin whiskers occurs in both
process (Lead Free and Tin Lead process)?
Thank you
_________________________
____
Juliano Bettim Ribeiro
DATACOM
ENGENHARIA DE PROCESSOS
Rua América Nº 1000 - Eldorado do Sul - RS CEP: 92990-000
+55 (51) 8446-2135
+55 (51) 3933-3000
Ramal: 3877
<mailto:[log in to unmask]> [log in to unmask]
<http://www.datacom.ind.br/> www.datacom.ind.br
_________________________
_________________________
____________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
_________________________
_________________________
____________________
***** Please note that my E-Mail address has changed *****
____________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please visit http://www.symanteccloud.com
____________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________