If your vendor contacts their ENIG vendor and requests a Palladium killer
cleaner that should take care of the plating in the non plated holes.
Usually the plating takes place in the hole due to presence of Pd left in
the hole. There are special cleaners designed to go after this Pd and
problem resolved.
Regards,
Bob Metcalf
Atotech Western Regional Manager
Cell 714-334-7667
E-Mail [log in to unmask]
This e-mail and any attachments hereto are business documents of Atotech
USA Inc. and may contain CONFIDENTIAL OR PROPRIETARY BUSINESS INFORMATION.
Unauthorized disclosure and/or use of information contained in this email
is prohibited. If you are not the intended recipient, you may not read,
use, disseminate or copy this message or any other files transmitted with
it.
From: David Hillman <[log in to unmask]>
To: <[log in to unmask]>
Date: 06/10/2014 10:07 AM
Subject: Re: [TN] Plating in non-plated holes - again
Sent by: TechNet <[log in to unmask]>
Hi Henry - maybe I am making this too simple but if your drawing/design
data shows a nonplated thru hole, then having any plating in it, partial
or
complete, is a violation of the drawing and therefore a nonconformance.
Dave
On Tue, Jun 10, 2014 at 10:26 AM, Henry Rekers <
[log in to unmask]> wrote:
> Hey there technetters. A while back, I sent a message about enig
plating
> contamination in NON-plated holes. I've bounced it back to the board
> shop saying that it is unacceptable, but they claim it is due to 6012
> 3.5.2
> I also think it's unacceptable in the 4552 spec. The design
> documentation clearly states non-plated. It's not plated, just
partially
> plated.
>
> Any advice?
>
> Thanks.
>
>
_____________________________________________________________________________________
>
>
> Henry Rekers P. Eng | Schneider Electric | Global Supply Chain |
> Senior Manufacturing Engineer
> Phone: +1-250-652-7100 ext. 7510 | Toll Free: +1-866-466-7627 ext.
> 7510 | Fax: +1-250-544-2390 |
> Email: [log in to unmask] | Site:
> www.schneider-electric.com | Address: 2195 Keating Cross Road,
> Saanichton, BC, Canada, V8M 2A5
> *** Please consider the environment before printing this e-mail
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
service.
> For more information please contact helpdesk at x2960 or
[log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|