TECHNET Archives

June 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ed Popielarski <[log in to unmask]>
Date:
Wed, 18 Jun 2014 13:45:06 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Bush, Brien" <[log in to unmask]>
Message-ID:
Subject:
From:
"Bush, Brien" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (55 lines)
Hi Ed,
We depanelize our boards before conformal coat. For depanelizing mouse bites, as in your picture, we use a Hepco
Depanelizer model #1200-1. They have various blade sizes for different configurations.


 Brien Bush
Manufacturing Applications Specialist
Cirtronics corp.
Milford, N.H.



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ed Popielarski
Sent: Tuesday, June 17, 2014 6:42 PM
To: [log in to unmask]
Subject: [TN] Laser depanelization

Hi all,

One of our aerospace customers is requesting boards depanelized from support frames.

I looked into router, but the conformal coating tends to smear and will be a significant FOD issue later.

We are willing to invest in laser, however, the result is a bit of charring on the edge, not much of a surprise. Unfortunately, this example http://stevezeva.homestead.com/Capture.JPG was rejected on IPC-A-610-Rev E Para. 10.7.4 "Solder Mask Coating-Discoloration" "Burned or charred solder mask material.

In my opinion, this is not within the "spirit of the law" since there are no specific provisions for laser depanelization, only marking.

Anyone know of some way around this?

Ed Popielarski
Engineering Manager

[cid:[log in to unmask]]
                               970 NE 21st Ct.
                              Oak Harbor, Wa. 98277

                              Ph: 360-675-1322
                              Fx: 206-624-0695
                              Cl: 949-581-6601

       "It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design."
https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
WARNING: Export Control This message, including any attachments, may contain technical data within the definition of the International Traffic in Arms Regulations (ITAR), and subject to the Export Control Laws of the U.S. Government. Transfer of such information by any means to a foreign person, whether in the United States or abroad, without proper export authorization or other approval from the U.S. Department of State is prohibited.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2