TECHNET Archives

June 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, David Hillman <[log in to unmask]>
Date:
Tue, 10 Jun 2014 11:25:39 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Henry Rekers <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (96 lines)
That's what I think, but we're getting push back from the supplier and I 
was hoping to get more specific. 

Thanks.

_____________________________________________________________________________________ 


Henry Rekers P. Eng |   Schneider Electric   |  Global Supply Chain  |   
Senior Manufacturing Engineer
Phone: +1-250-652-7100 ext. 7510  |   Toll Free: +1-866-466-7627 ext. 
7510  |   Fax: +1-250-544-2390  |   
Email: [log in to unmask]  |   Site: 
www.schneider-electric.com  |   Address: 2195 Keating Cross Road, 
Saanichton, BC, Canada, V8M 2A5 
*** Please consider the environment before printing this e-mail



From:
David Hillman <[log in to unmask]>
To:
<[log in to unmask]>, 
Date:
06/10/2014 10:08 AM
Subject:
Re: [TN] Plating in non-plated holes - again
Sent by:
TechNet <[log in to unmask]>



Hi Henry - maybe I am making this too simple but if your drawing/design
data shows a nonplated thru hole, then having any plating in it, partial 
or
complete, is a violation of the drawing and therefore a nonconformance.

Dave


On Tue, Jun 10, 2014 at 10:26 AM, Henry Rekers <
[log in to unmask]> wrote:

> Hey there technetters.  A while back, I sent a message about enig 
plating
> contamination in NON-plated holes.   I've bounced it back to the board
> shop saying that it is unacceptable, but they claim it is due to 6012
> 3.5.2
> I also think it's unacceptable in the 4552 spec.   The design
> documentation clearly states non-plated.   It's not plated, just 
partially
> plated.
>
> Any advice?
>
> Thanks.
>
> 
_____________________________________________________________________________________
>
>
> Henry Rekers P. Eng |   Schneider Electric   |  Global Supply Chain  |
> Senior Manufacturing Engineer
> Phone: +1-250-652-7100 ext. 7510  |   Toll Free: +1-866-466-7627 ext.
> 7510  |   Fax: +1-250-544-2390  |
> Email: [log in to unmask]  |   Site:
> www.schneider-electric.com  |   Address: 2195 Keating Cross Road,
> Saanichton, BC, Canada, V8M 2A5
> *** Please consider the environment before printing this e-mail
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud 
service.
> For more information please contact helpdesk at x2960 or 
[log in to unmask]
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2