TECHNET Archives

June 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Date:
Wed, 4 Jun 2014 20:27:35 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Thierolf, Chris @ MPSG - SPD" <[log in to unmask]>
Message-ID:
Subject:
From:
"Thierolf, Chris @ MPSG - SPD" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (57 lines)
I'm assuming you are referring to the drill tooling that requires sensors and instrumentation. Halliburton and Sperry are leaders in this area. http://www.halliburton.com/en-US/ps/sperry/drilling/geosteering-services/gabi-downhole-drilling-motor.page

Temperatures can reach close to 200C under very high pressure while subjected to gases and fluids. This article may help

http://globalpetroleumshow.com/wp-content/uploads/sites/2/ElectronicParts_JPT_Aug13.pdf



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Wednesday, June 04, 2014 3:51 PM
To: [log in to unmask]
Subject: Re: [TN] high temp environment

What temperatures will the device see (both external and internal) in the field?
There are companies that make equipment for monitoring lava temperatures. If they can do that, then the inside of an oil well should be pretty ho hum.....

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
Sent: Wednesday, June 04, 2014 2:19 PM
To: [log in to unmask]
Subject: [TN] high temp environment

Hello Technet!
We are discussing an opportunity with a customer who is looking at placing an instrument down-hole in an oil well, hence a high temp environment.  Are there any good resources around to help me with this one?  Obviously I need high temp solder (Sn96Ag4?), the components will have to be carefully picked, and we will need PWBs that will be OK at high temp (polyimide?).

I've got some homework to do! :-)

--
regards,

Graham Collins
Senior Process Engineer
Sunsel Systems
(902) 444-7867 ext 211


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
________________________________
CONFIDENTIALITY NOTE: This electronic transmission, including all attachments, is directed in confidence solely to the person(s) to whom it is addressed, or an authorized recipient, and may not otherwise be distributed, copied or disclosed. The contents of the transmission may also be subject to intellectual property rights and all such rights are expressly claimed and are not waived. Unless specifically modified by L-3 SPD Electrical Systems , the content of this electronic transmission is to be read subject to L-3 SPD Electrical Systems  standard terms of business. This electronic transmission may be intercepted or affected by viruses and L-3 SPD Electrical Systems  accepts no responsibility for any interception or liability for any form of viruses introduced by this electronic transmission. If you have received this transmission in error, please notify the sender immediately by return electronic transmission and then immediately delete this transmission, including all attachments, without copying, distributing or disclosing same.

ITAR CONTROL STATEMENT:

In the event this document (or any of the enclosures) contains technical data within the definition of the International Traffic in Arms Regulations or Export Administration Regulations, it is subject to the export control laws of the U.S. Government. Transfer of this data by any means to a foreign person, whether in the United States or abroad, without an export license or other approval from the U.S. Department of State or Commerce, is prohibited.


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2