TECHNET Archives

June 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 24 Jun 2014 14:58:31 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Message-ID:
Subject:
From:
Wayne Thayer <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (303 lines)
So your environment is pretty much the same as the engine compartment of a 
motorboat powered with gasoline.

If you look at how they design the alternator for that environment, they just 
assume it's going to spark, and put grounded screens/cages around any place 
that could be susceptible to sparking.  Strangely, things seem to be OK with 
the exposed spark plug wires, although there are several boat explosions due 
to this problem every year--it's not like the FAA accident investigation, even 
though at least a few people die due to this every year.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Monday, June 23, 2014 7:22 PM
To: [log in to unmask]
Subject: Re: [TN] z-axis voltage separation

Curt,

 Thanks, yes I have been through these issues but a second read is always a 
good idea. Some of my docs are real old.

 The hazardous locations I am working in is a room filled with explosive 
vapors. One spark and it is a real problem!

 I need an isolation transformer that feeds power from one side to an isolated 
secondary. The coil needs to be physically small as there are limits to the 
power I can allow through during fault conditions. But small transformers make 
insulating difficult.  I am working with an EFD10 which is rather tiny, only 2 
or 3 watts can ever go through that tiny magnetic circuit.

 Normally both transformers sides are at a common earth ground. But with a 
power system faults GND ain't GND anymore. I have not been able to locate docs 
on how to define this event so I am looking for as much side to side isolation 
as I can. The optos in the system are rated at 3750VAC so I figure I want to 
be a little better than the optos.

 Using Quad Build wire I get over 6KV on each wire and a single layer of tape 
gets me 6KV. But I would like to establish a safety margin but I have no idea 
what is a reasonable safety margin number. Is it 10%, 100% or 500%?

 I can measure to 6KV here, and I think that is plenty, but with a reasonable 
margin what should I spec?

Thanks,
Bob K.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Curt McNamara
Sent: Monday, June 23, 2014 5:35 PM
To: [log in to unmask]
Subject: Re: [TN] z-axis voltage separation

Maybe this will help, apologies if you know all of it!

A hazardous design (i.e. one that has high voltages in it) needs to meet the 
relevant safety standard. The appropriate standard is determined by the market 
and the end use of the design. For example, IT equipment typically has to meet 
60950, while laboratory equipment may need to meet 61010. There are many many 
standards.

To get an approval, the safety agency will do an analysis of the design by 
examining the components, including the PCB.

If a component (like an insulator, transformer, or fuse) has UL Recognition 
then that qualification can be used in the final design.

If a component (like a PCB) does not have UL recognition (and PCBs don't) then 
it needs to meet Creepage and clearance as defined in that standard.

If the component (like the PCB) does not meet creepage and clearance, then 
each individual instance will need to be hi-pot tested.

This is a reasonable overview of the material:
http://www.springer.com/cda/content/document/cda_downloaddocument/9781461410522-c1.pdf?SGWID=0-0-45-1298737-p174268563

		Curt

Curt McNamara, M. Eng. P.E.  //  principal electrical engineer | electrical 
engineering

Logic PD
411 Washington Ave. N. Suite 400
Minneapolis, MN 55401
T // 612.436-5178
NOTICE: Important disclaimers and limitations apply to this email.
Please see this web page for our disclaimers and limitations:
http://logicpd.com/email-disclaimer/


-----Original Message-----
From: Robert Kondner [mailto:[log in to unmask]]
Sent: Monday, June 23, 2014 4:06 PM
To: 'TechNet E-Mail Forum'; Curt McNamara
Subject: RE: [TN] z-axis voltage separation

Curt,

 But thickness matters too!  I recall the UL double insulated requirement is 
only about 7 mil thick insulation. Do I remember that correctly?

 I think they call this a dielectric withstanding rating.

 A quick look at my old UL 478 spec shows a 250 VAC must withstand 1250V. Now 
that you can propably do with a single layer of Scotch Tape. I would not 
consider that very safe. Even a single layer of transformer tape (polyester) 
does not strike me as "Safe".

There are "Resistance Measurements" for items, they soak at specific humidity 
levels and then the resistance is checked. But this highest withstanding 
voltage I see at any level is only 3000V. That is all Class II, Class I is 
much less.

Summary: There really is no "Safety Margin" to speak of, we need only meet 
insulation tests and fairly low (3000V worse case) for UL 478 type items.

I have been looking at some hazardous location specs which have their own 
clearances but withstanding voltages is all I have to go on for HV isolation 
in small power supplies.

Anyone out there really know this subject?

Thanks,
Bob K

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Curt McNamara
Sent: Monday, June 23, 2014 4:08 PM
To: [log in to unmask]
Subject: Re: [TN] z-axis voltage separation

As others have noted, voltage isolation spacings are defined by Creepage and 
clearance requirements in the relevant safety standard. 3.5mm seems about 
right. If you move the traces far enough away in X or Y you should be able to 
meet the spacing requirements.

As Wayne notes, FR4 is not a consistent insulator, as its' properties vary 
from build to build (plus there could be copper in there!).

A PCB could be designed, built, and pass a safety examination with spacing 
violations (since FR4 will insulate), however each PCB will then need to be 
hi-pot tested to meet the standard.

		Curt

Curt McNamara, M. Eng. P.E.  //  principal electrical engineer | electrical 
engineering

Logic PD
411 Washington Ave. N. Suite 400
Minneapolis, MN 55401
T // 612.436-5178
NOTICE: Important disclaimers and limitations apply to this email.
Please see this web page for our disclaimers and limitations:
http://logicpd.com/email-disclaimer/


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer
Sent: Monday, June 23, 2014 2:44 PM
To: [log in to unmask]
Subject: Re: [TN] z-axis voltage separation

Surface flash and arcing in air are pretty well understood, but there are 
large fudge factors for shape and humidity and contamination.

Breakover inside a dielectric which isn't fundamentally designed as a high 
voltage material and consists of a bunch of fibers with resin filler has a 
bunch of interesting failure modes, some of which take a long time to happen.

As has been suggested, you could get insignificant tiny arcs from fiber to 
fiber which would eventually result in a "tree-like" failure in the material.

If you need high voltage high reliability in a dielectric, the material has to 
be qualified via HAST in the usage condition.  Manufacturers do sell 
pre-qualified materials--FR4 isn't one of them.

So starting with surface flash criteria is one way to look at it, but I think 
that is pretty darn conservative on it's own.  I wouldn't add extra factors, 
and you could probably go higher stress than that safely.

But as I previously indicated, go with CAF resistant material and go extremely 
conservative if there's a plated through-hole near by.

And that's all you get for a nickel!

Wayne

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Monday, June 23, 2014 1:49 PM
To: [log in to unmask]
Subject: Re: [TN] z-axis voltage separation

Ahne,

 You mentioned "I would put in a generous safety factor"

 I have been looking for a realistic "Safety Factor" for some small high 
isolation voltage coils. Any idea how "Safety Factors" are computed? Are 
safety factors just wild guesses for engineers to make up themselves?

Thanks,
Bob K.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ahne Oosterhof
Sent: Monday, June 23, 2014 12:54 PM
To: [log in to unmask]
Subject: Re: [TN] z-axis voltage separation

After a long search,
http://advancedmaterialscience.com/products/NEMA%20FR4.pdf
Dielectric strength:  550 volts/mil

An example (from a vendor).
Semi-Flex FR4, 2 Layers Prototype PCB FR4, 0.3mm Thick Board thickness: 0.3mm 
Electric strength: >1.3kv/mm

Dupont Pyralux: Dielectric Strength,  ASTM-D-149,  6-7 kV/mil

FR4 is not a homogenous material, so I expect that the dielectric strength for 
thinner layers will be lower than for thicker layers. And if you measure it, I 
would put in a generous safety factor.
Many vendors provide some kind of number for dielectric strength, but rarely 
add the complete description of and conditions under which the material was 
tested.

If your concern is rooted in safety you will end up testing it yourself for UL 
(or something like that) approval.

Have fun,
Ahne.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: Friday, June 20, 2014 8:38 AM
To: [log in to unmask]
Subject: [TN] z-axis voltage separation

maybe I'm having a "not enough coffee yet" morning, but I was asked how much 
separation I need between layers for high voltage.
I tried to search the TechNet Archives, but it doesn't seem to work as well as 
it used to!
anyway,

We have a design that may have 1700V in several places.
Since we are looking at a clearance into the board, layer-to-layer I'm pretty 
sure I can use the "internal" column B1 of Table 6-1 in IPC-2221 (using Table
6-1 for z-axis was discussed in an IPC committee meeting and no one disagreed)

but the number I get for 1700V is =
(.25 mm for the first 500V) plus (.0025 mm for each of the other 1200V, 3
mm)
equals 3.25 mm

For one thing, it already seems like I'm off-track because .25 for 500V 
doesn't correspond very well with 3 mm for 1200V, but if you can't trust 
IPC..... well, let's not go there.

My REAL question is that, although I'm safe using 3.25 mm, my board is not 
that thick!
Is there a smaller z-axis clearance that can be used for 1700V? across typical
FR4 material?
(we are using a RoHS compatible 170Tg /126)

What's the MINIMUM layer spacing I can use for 1700V?

thanks,
Jack


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2