Gregg:
A CO2 laser will ablate in a very precise fashion followed by a clean up
operation.
Bob Wettermann/BEST
On Thu, May 1, 2014 at 1:53 PM, Gregg Owens <[log in to unmask]> wrote:
> Anyone know of an easy way to remove Kapton insulation from solid 26AWG
> wire? We have to prep such wires for soldering. I thought we could simply
> remove with a solder pot but the insulation is just too resilient. Any
> ideas?
>
> Thanks,
>
> Gregg
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
--
Bob Wettermann
BEST Inc
[log in to unmask]
Cell: 847-767-5745
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________