Wow, it seems Technet has been very quiet lately.....so here is a question I faced yesterday:
Our PWA assembly process uses solder paste which contains flux classified as ORHO (for SMT).
We clean using DI water afterwards. Then we hand install non-SMT components using core solder containing ROL0 flux and liquid flux classified as ROL1, and clean afterwards using alcohol (I know, I know).
During an audit, it was questioned whether or not we are in compliance with J-STD-001E Section 3.3 for compatibility.
My question to all of you is what does "data demonstrating compatibility" actually mean?
Is this compatibility between different fluxes, or between residues, or .....?
"3.3 Flux
Flux shall [D1D2D3] be in accordance with J-STD-004 or equivalent.
Flux shall [N1N2D3] conform to flux activity levels L0 and L1 of flux materials rosin (RO), resin (RE), or organic (OR),
except ORL1 shall not [N1N2D3] be used for no-clean soldering.
When other activity levels or flux materials are used, data demonstrating compatibility shall [N1N2D3] be available for
review (see 3.1).
Note: Flux or solder paste soldering process combinations previously tested or qualified in accordance with other specifications
do not require additional testing."
________________________________
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|