TECHNET Archives

May 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 23 May 2014 14:54:20 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steven Kelly <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
<52135AE4151D8343B16989B2BFBED7DA3831317F3E@pfc-dc01>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Steven Kelly <[log in to unmask]>
Parts/Attachments:
text/plain (9 lines)
Hi All,
Can someone explain to me why in a SEM/EDX analysis of a solder joint there would be Oxygen?
Thanks Steve Kelly