TECHNET Archives

April 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
[log in to unmask], "Thierolf, Chris @ MPSG - SPD" <[log in to unmask]>
Date:
Tue, 8 Apr 2014 17:21:15 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Steve Gregory <[log in to unmask]>
Parts/Attachments:
text/plain (82 lines)
Hi Chris,

Just throwing this out there. I don't know what kind of package you're
dealing with, you said 4-leads, could it be one like this?

http://media.digikey.com/photos/Allegro%20Microsystems/A1233LK-T.JPG

I know a solder joint is better than a socket, but maybe something to
consider is something like this:

http://documents.tycoelectronics.com/commerce/DocumentDelivery/DDEContro
ller?Action=showdoc&DocId=Specification+Or+Standard%7F114-13033%7FA%7Fpd
f%7FEnglish%7FENG_SS_114-13033_A.pdf


Steve 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Thierolf, Chris @
MPSG - SPD
Sent: Tuesday, April 8, 2014 1:01 PM
To: [log in to unmask]
Subject: [TN] Reattachment of leads

Is anyone familiar with the re-attachment of leads to a through hole
package when the original leads were cut? I have a very hard to find
package that had leads cut half length in attempts to make surface
mountable and want to add 4 leads to desired length. We tried a
resistance weld process through a vendor to fuse the leads together but
upon solder reflow the leads fell apart. I suspect thermal expansion or
insufficient bonding to be the cause under heat so I need an optional
process. Any ideas? The leads are tinned copper.

thanks

______________________________________

Chris Thierolf


________________________________
CONFIDENTIALITY NOTE: This electronic transmission, including all
attachments, is directed in confidence solely to the person(s) to whom
it is addressed, or an authorized recipient, and may not otherwise be
distributed, copied or disclosed. The contents of the transmission may
also be subject to intellectual property rights and all such rights are
expressly claimed and are not waived. Unless specifically modified by
L-3 SPD Electrical Systems , the content of this electronic transmission
is to be read subject to L-3 SPD Electrical Systems  standard terms of
business. This electronic transmission may be intercepted or affected by
viruses and L-3 SPD Electrical Systems  accepts no responsibility for
any interception or liability for any form of viruses introduced by this
electronic transmission. If you have received this transmission in
error, please notify the sender immediately by return electronic
transmission and then immediately delete this transmission, including
all attachments, without copying, distributing or disclosing same.

ITAR CONTROL STATEMENT:

In the event this document (or any of the enclosures) contains technical
data within the definition of the International Traffic in Arms
Regulations or Export Administration Regulations, it is subject to the
export control laws of the U.S. Government. Transfer of this data by any
means to a foreign person, whether in the United States or abroad,
without an export license or other approval from the U.S. Department of
State or Commerce, is prohibited.



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2