Erbium (Er) is my guess.
Leland
________________________________________
From: TechNet [[log in to unmask]] on behalf of David D. Hillman [[log in to unmask]]
Sent: Friday, March 14, 2014 10:29 AM
To: [log in to unmask]
Subject: [TN] NTC Element Quiz Question
Hi folks - Here is the Element Quiz Question:
The Question:
This element is one of the REEs. You refine one million pounds of the
Earth's crust to yield 2.5 pounds of this element. It is alloyed with
vanadium to form spring steel. It is magnetic at very low temperatures.
What element is being described?
The winner of the weekly element quiz will get the services of Clumpy and
Kloumpios for the week.
So far Clumpy and Kloumpios have done the following:
Past Quiz winners/tasks:
Week 1 Dick Krug, Spartan Complex Systems
Week 2 Laura Turbini, IRC
Week 3 James Head, Crowcon Detection Instruments Limited
Week 3 Pat Goodyear, PGE
Week 4 Joe Russeau, Precision Analysts Laboratory
Week 5 Tom Carroll, Boeing Defense, Space and Security
Week 6 Steve Gregory
Week 7 Phil Kinner
Week 8 Brian Ellis
Week 9 James Head, Crowcon Detection Instruments Limited
Week 10 Leland Woodall, CSTech Inc.
Week 11 Keith Calhoun, Sopark Corp
Week 12 Matthias Mansfeld, Mansfeld-Elektronik
Week 13 Leland Woodall, CSTech Inc.
Week 14 Brian Ellis
Week 15 Tom Carroll, Boeing Defense, Space and Security
Week 16 Steve Gregory
Week 17 Phil Kinner
Week 18 Ian Braddock, MBDA Systems
Week 19 Leland Woodall, CSTech Inc.
Week 20 Denny Fritz, SAIC
Week 21 Amol Kane
Week 21 Dewey Whittaker, Honeywell
Week 21 David Bealer, Watch Fire Signs
Week 22 Phil Kinner
Week 23 Guy Ramsey, RD Circuits
Week 24 Mark Kostinovsky, Schlumberger
Week 25 Keith Calhoun, Sopark Corp
Week 26 Paul Reid, PWB Interconnect Solutions Inc
Week 27 Greg Munie, IPC
Week 28 Steve Gregory
Week 29 Gus Trakas, Viasystems
Week 29 Steve Creswick
Week 30 Robert Welch, Moog Component Group
Week 31 Heidi Havelka, Interplex Sunbelt
Week 32 Raye Rivera, Canoga Perkins
Week 33 Steve Creswick
Week 34 Dewey Whittaker, Honeywell
Week 35 Don Vischulis
Week 36 Greg Munie, IPC
Week 37 Larry Dzaugis
Week 37 Bonus Question Steve Mikell
Week 38 Curt McNamara, Logic PD
Week 38 Bonus Question Dewey Whittaker, Honeywell
Week 39 Leland Woodall, CSTech Inc.
Week 40 Leland Woodall, CSTech Inc.
Week 40 Ron Feyereisen, Sigmatron Int.
Week 41 Steve Gregory
Week 42 Steve Mikell
Week 43 Mark Kostinovsky, Schlumberger
Week 44 Leland Woodall, CSTech Inc.
- I've got some very important work for the boys this week. I'm going to
ask them to submerge several piles of brush in our local reservoir in
anticipation of the upcoming Spring crappie fishing season.
Week 44 Eddie Hofer, Rockwell Collins
- I think I'll have them practice a little baseball & hockey with my son
this week so I don't have to put on the skates or baseball glove.
Week 45 Leland Woodall, CSTech Inc.
- Rumor has it Leland's facility had an ice storm so the boys put their
salt spreader attachments on their tractors and should
be at his place today to assist.
Week 46 Joe Russeau, Precision Analysts Laboratory
- assisted with ????
Week 47 ????
- assisted with ????
Everyone have a safe week.
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
________________________________
“Confidentiality Notice:
This transmission (including any attachments) may contain confidential information belonging to the sender and is intended only for the use of the party or entity to which it is addressed. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution, retention or the taking of action in reliance on the contents of this transmission is strictly prohibited. If you have received this transmission in error, please immediately notify the sender and erase all information and attachments.”
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|