Check kester. It has fair amount of work done too.
Joyce Koo
Researcher
Materials Interconnect Lab
Office: (519) 888-7465 79945
BlackBerry: (226) 220-4760
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Monday, March 10, 2014 9:29 AM
To: [log in to unmask]
Subject: Re: [TN] Fluxing Underfills
Back around 12-15 years ago the Universal Instruments Area Array consortium was doing quite a bit of work on this topic.
Most of their immediate work is for consortium members only, but I think it is made public after 5 years.
I recall attending several presentation on this topic.
Rich Kraszewski
PLEXUS
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Greg Munie
Sent: Friday, March 07, 2014 1:55 PM
To: [log in to unmask]
Subject: [TN] Fluxing Underfills
Anyone have any experience with fluxing underfills?
How well do they work on larger bumped packages?
Are they repairable?
The question came up here at IPC but I've been out of the flux business too long to answer.
Greg Munie Ph.D.
Director of Design Programs
+1-847-616-7100 tel
+1-847-597-2803 direct
[log in to unmask]<mailto:[log in to unmask]>
www.ipc.org<http://www.ipc.org/>
[cid:[log in to unmask]][http://www.ipc.org/images/shim.gif]<http://www.ipc.org/>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________