Have to agree with Lloyd, that looks suspiciously like parylene (or some
sort of coating). Virgin MIL-38999 connectors don't look like that...
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of lduso -
Diamond-MT.com
Sent: Tuesday, March 11, 2014 10:22 AM
To: [log in to unmask]
Subject: Re: [TN] Connector Mating Surface Flashing
It resembles a connector that has been parylene coated and the remnants
of parylene after the holes were punched.
Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com
On Tue, Mar 11, 2014 at 12:13 PM, McGlaughlin, Jeffrey A <
[log in to unmask]> wrote:
> This appears to be the insert on a circular connector, so it should
> have a related MIL SPEC to reference. Try MIL-STD 1560 or MIL-STD-1669
> as source to find the correct workmanship standards. Are these suppose
> to be sealed connectors? I ask because the flashing appears to be a
> different material than the phenolic insert. Regardless, I would not
> accept connectors like this as this is an obvious workmanship issue.
>
> Jeffrey McGlaughlin, C.I.D.
> Engineering Designer
>
> Battelle
> 505 King Avenue
> Columbus Ohio 43201-2693
> [log in to unmask]
>
> This message is intended only for the use of the individual or entity
> to which it is addressed, and may contain information that is
> privileged, confidential and/or otherwise exempt from disclosure under
applicable law.
> If the reader of this message is not the intended recipient or the
> employee or agent responsible for delivering the message to the
> intended recipient, any disclosure, dissemination, distribution,
> copying or other use of this communication or its substance is
> prohibited. If you have received this communication in error, please
> return to the sender and delete from your computer system.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Joseph E (US
> SSA)
> Sent: Tuesday, March 11, 2014 8:08 AM
> To: [log in to unmask]
> Subject: [TN] Connector Mating Surface Flashing
>
> My coworker Thomas Cleere has posted a picture titled "Connector with
> Flashing" to the photo site at:
>
> www.ipc.org/technet-photos<http://www.ipc.org/technet-photos>
>
> I'll also send a copy to Steve.
>
> Anyone seen anything like this? Obviously, our concern is that the
> excess material will get stuffed down the hole during the mating
> action, and cause an open.
>
> IPC/WHMA-A-620 only cover cracks or tears in this surface, and 610
> doesn't address it at all, are any criteria established elsewhere?
>
> Joe Kane
> BAE Systems
> Endicott, NY
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|