TECHNET Archives

March 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Don Vischulis <[log in to unmask]>
Date:
Fri, 28 Mar 2014 19:31:31 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Message-ID:
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (67 lines)
Don,
I'm trying to get a pin analyzed now. I was just asking if any old or young experts had some insight/opinion on the situation so I could argue/justify the additional research needed to correctly address the problem.
Thanks,
Dewey 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Don Vischulis
Sent: Friday, March 28, 2014 12:18 PM
To: [log in to unmask]
Subject: Re: [TN] Pins and Needles

If a sample is available som lab work to analyze the materials might be helpful. Probably beryllium copper for the pins. Silver thickness will affect reliability. 

Don Vischulis
Sent from my iPhone

> On Mar 28, 2014, at 11:16 AM, Patrick Goodyear <[log in to unmask]> wrote:
> 
> Dewey,
> 
> More detail would be needed, old product name....   Was it Mil-spec? etc.    I am an old tech but don't remember seeing such an animal.   The silver plate was most likely used because silver oxide is has a high conductivity, I think right next to copper but not as soft and the pin, may have been copper-beryllium, since that is a common usage for some tooling and most likely silver plated directly on.   Check Keystone Electronics to see if they have anything in their archives.   Silver over brass and bronze were very common for Mil-Spec equipment.
> 
> Pat Goodyear
> Semi-retired Control Technician
> 
>> On Fri, Mar 28, 2014 at 7:37 AM, Whittaker, Dewey (EHCOE) wrote:
>> 
>> Dear Technet,
>> For the record I'm looking for a special talent. Old, old product that has beryllium pins ultrasonically bonded in a plastic switch housing. The pin is silver plated prior to installation. The spec  and materials have been obsolete for 25-30 years. They asked me to write a new one, so my first question was why silver? Watching too many Lone Ranger episodes as a child or hooked on oxides?
>> One end of the pin rubs on the sliding switch plate (proprietary 
>> finish) which is probably silver. The other end of the pin is installed in a PBA and flow soldered .
>> So the pin has to be conductive, solderable and let's say hard. There is  no specific information on the beryllium pin, so how do I help them without knowing how I helped them. My questions are as follows:
>> 
>> *         Do I apply a copper plate on the pin first
>> 
>> *         Do I apply  a nickel barrier layer over the copper plate
>> 
>> *         What nickel plating spec (ASTM B 700) do I use and what minimum thickness (200-300 micro-inches) when one end needs to be soldered
>> 
>> *         Should the solder in the flow solder bath be 2% Ag
>> I would not have designed this  is and what I want to change it may not be possible, I'm open to suggestions to try anyway. Whole new pin with one special surface finish, would be my reply.
>> 
>> Dewey
>> 
>> _____________________________________________________________________
>> _ This email has been scanned by the Symantec Email Security.cloud 
>> service.
>> For more information please contact helpdesk at x2960 or 
>> [log in to unmask] 
>> _____________________________________________________________________
>> _
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2