TECHNET Archives

February 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Ed Popielarski <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ed Popielarski <[log in to unmask]>
Date:
Mon, 10 Feb 2014 23:04:58 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (48 lines)
FOD resulting from working one's fingers to the bone.

Ed Popielarski
Engineering Manager


                               970 NE 21st Ct.
                              Oak Harbor, Wa. 98277

                              Ph: 360-675-1322
                              Fx: 206-624-0695
                              Cl: 949-581-6601

https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Monday, February 10, 2014 2:08 PM
To: [log in to unmask]
Subject: [TN] Risks Associated with Calcium

I am occasionally seeing irritating low levels of calcium in some assemblies that we test via ion chromatography.

Some organizations required spec levels as low as <1 ppm.

My questions to you techies is:

#1 Besides wash water are there any other sources of calcium that come to  mind?

#2 is there any real value in having Calcium specs down as low as 1 ppm?  (I suspect not and this spec was merely carried over from the semiconductor industry where it may have more value)

CH65 is of some help here in that is does speak much more of the evils of Na that Ca& Mg, but not as much as I had hoped. 

Thoughts??

Rich  Kraszewski
Senior Process Engineer
Plexus Engineering Solutions 

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2