Are you supposed to clean each individual 0402 part? Zoiks!
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, February 20, 2014 12:27 PM
To: [log in to unmask]
Subject: Re: [TN] Acetone as a cleaning agent for PCBA's
Hi Bob,
It's funny you should mention that. We're looking at building a board that contains these little devices from Avago that says to clean with with Acetone and rinse with Alcohol:
http://www.avagotech.com/docs/AV02-2001EN
I've never had to do that before. Hmmmmm....
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert DeQuattro
Sent: Thursday, February 20, 2014 10:00 AM
To: [log in to unmask]
Subject: [TN] Acetone as a cleaning agent for PCBA's
I have a customer that uses acetone to wipe down their PCBA's upon receipt.
The assemblies we make for them are cleaned using a closed loop aqueous board washer then sampled for cleanliness with our zero-ion tester per J-std-001E guidelines.
Recently this customer commented that boards appeared dirty upon cleaning with the acetone. Does anyone have any thoughts on this acetone cleaning process.
Thanks,
Bob
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|