Hello technetters....
One of our plants is trying to implement an automated conformal coating
process and we are running into some issues with our material. It seems
that the coating is "bouncing" off the board and splattering over the rest
of the board.
My first thought, probably just like yours, is too much air pressure. But,
does the collective have any other suggestions?
The material is humiseal 1a33, it's thinned with humiseal 521 (60:40) and
it's and SCS coating machine.
Thanks in advance.
_____________________________________________________________________________________
Henry Rekers P. Eng | Schneider Electric | Global Supply Chain |
Senior Manufacturing Engineer
Phone: +1-250-652-7100 ext. 7510 | Toll Free: +1-866-466-7627 ext.
7510 | Fax: +1-250-544-2390 |
Email: [log in to unmask] | Site:
www.schneider-electric.com | Address: 2195 Keating Cross Road,
Saanichton, BC, Canada, V8M 2A5
*** Please consider the environment before printing this e-mail
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|