Lars,
In my working career we had issues with a SCR mounted in a heat sink
bolted to a single sided board much like C, normal cycling not sure how
many but over 10 years the solder would crack at the lead land juncture.
So with that in mind I would say the best solution is, B, however the
leads may break at the component. If you could keep the poly out
from under the cap would be best. Next best would be to incorporate
stress relief between the base of the cap and the board and stand the
cap off the board slightly, using the poly to support the cap weight.
It also matters whether the cap is mounted vertical or horizontal in
relation to gravity. We had a group of boards edge mounted in a card
cage and the large block caps fell off of the boards over time, 50 or so
of them. Ended up replacing that type and using RTV to support them.
pat
On Thu, Feb 6, 2014 at 5:14 AM, Lars Wallin wrote:
> Hello Technet,
>
> Please check the attach sketch.
> It involves soldering a large capacitor (20 x 30 x 40 mm see enclosed
> picture) and then mould in the whole board with a warm polyuretan
> mould mass. The requirement is that the solder joint should withstand
> 300 cycles (from-40C to +85 C).
>
> Figure A, can not cope with the requirement of 300 cycles. a =
> polyurethane mass.
>
> Which of the figures B-E do you think would be a better solution? Or
> would you suggest any other solution?
>
> Looking forward to your answer.
>
> Best Regards
> Lars Wallin
> IPC European Representative
> Location: Stockholm, Sweden
> Phone: +46 8 26 10 07
> Mobile: +46 70 212 74 39
> Email: [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|