TECHNET Archives

February 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 3 Feb 2014 17:47:59 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, GRIVON Arnaud <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
GRIVON Arnaud <[log in to unmask]>
Parts/Attachments:
text/plain (18 lines)
Hello TechNet,

I would like to sense the best practices in terms of solder mask surface tension with respect to conformal coating adhesion :

-          Which standard/test method are you using?

-          Which requirement (e.g. minimum value in dyn/cm²) would you accept for the various CC types (acrylics, urethanes, silicone, parylene)?
Thanks in advance for the insights.
Best regards,

Arnaud Grivon


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2