Subject: | |
From: | |
Reply To: | |
Date: | Mon, 6 Jan 2014 16:10:19 -0600 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Good afternoon all,
I need help finding an adequate term for something, so I thought I would
ask you all.
If I am inspecting conformal coating, and I see a visual "item of
interest", what term generically do I call the "item of interest"? The
item of interest may or may not be a defect but it looks visually
different than the coating around it.
I have tried Visual Anomaly, or Visual Artifact, but people here don't
seem to like any of them?
What do y'all think?
Doug Pauls