TECHNET Archives

January 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 14 Jan 2014 14:14:53 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, David Quiroz <[log in to unmask]>
Message-ID:
Subject:
From:
David Quiroz <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (100 lines)
Thanks for the input, gentlemen.

DQ

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of colin mcvean
Sent: Monday, January 13, 2014 11:24 AM
To: [log in to unmask]
Subject: Re: [TN] Brushes for Use in PCB Lamination Area


David,

I agree with Roberts conclusion: best practice is vacuum either central
based system or stand-alone with Hepa filter after each lay-up of book or
surrounding area and use of tacky roller with adhesive pads or interleavers
and core layers. Don't use this on the prepreg though, and be careful not to
remove or damage any of the oxide or bond adhesion film on the core layers.
Best to roller one side flat, then place face down onto the stack then
roller the second side. It take a bit of organisation, but risk of FOD is
greatly reduced.

Consider also, stacking of materials in a rack system, with cleanest
material at top, like the copper foil, then cores then prepregs at bottom -
saves clean materials being contaminated with falling particles and dust. As
for copper foils, buy this in shiny to shiny, which save additional handling
and potential damage.

Colin



On Monday, 13 January 2014, 18:13, Robert F. Bagsby
<[log in to unmask]> wrote:

Hi David,

Brushing tends to move dust, debris, particular matter around and not
actually pick it up.  Depending on the vigorousness of the action, can
actually cause the stuff you're trying to brush away to go places you
don't want it (into the setup perhaps).  I recommend more of a clean room
practice of vacuuming (central vac system) or a clean room hand tacky
roller with sticky pad, or web cleaner.  Organization of the lay-up
station can help minimize transfer of material of one type to another (say
prepreg dust onto copper foil, leading to resin spots)  or (slivers from
pre-tooled copper foil into prepreg, leading to shorts).



Robert F Bagsby / Manager, Project & Technical Services / Projects,
Technical Services & Lean
MS 130-108, Cedar Rapids, IA, 52498, USA
Phone: 319-295-8703 / VPN: 295-8703 / Mobile: 319-573-6859
[log in to unmask]
www.rockwellcollins.com




From:   David Quiroz <[log in to unmask]>
To:     <[log in to unmask]>
Date:   01/13/2014 10:26 AM
Subject:        [TN] Brushes for Use in PCB Lamination Area
Sent by:        TechNet <[log in to unmask]>



Hello All,

Can anyone recommend a good quality hand brush that can be used in a pcb
lamination layup area?  I'd like to use it for brushing off
plates/panels/foil during layup of lamination books.

Regards,
David Quiroz


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2