I believe that Kovar alloys are tempered as part of their material treatment. Does this imply that all Kovar based leads, which are widely used on standard TH DIL's can not be clinched or cut ?
Regards
Bryan Kerr
Principal Quality Engineer
CMA Lab and Process Engineering
BAE Systems Maritime Services
Manufacturing Hillend
Hillend Industrial Estate
Hillend
Nr Dunfermline
Fife
Scotland
KY11 9HQ
01383-836097
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kerr, Bryan (UK)
Sent: 28 January 2014 12:07
To: [log in to unmask]
Subject: [TN] Tempered leads
----------------------! WARNING ! ---------------------- This message originates from outside our organisation, either from an external partner or from the internet.
Consider carefully whether you should click on any links, open any attachments or reply.
Follow the 'Report Suspicious Emails' link on IT matters for instructions on reporting suspicious email messages.
--------------------------------------------------------
Hi All
IPC spec's have requirements on clinching and cutting of "tempered leads". Can anyone advise me of the typical components which would have such leads ? Also, would these always be iron based alloys ?
Regards
Bryan Kerr
Principal Quality Engineer
CMA Lab and Process Engineering
BAE Systems Maritime Services
Manufacturing Hillend
Hillend Industrial Estate
Hillend
Nr Dunfermline
Fife
Scotland
KY11 9HQ
01383-836097
********************************************************************
This email and any attachments are confidential to the intended recipient and may also be privileged. If you are not the intended recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or distribute its contents to any other person.
********************************************************************
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|