By the way, I'll wager that 85/85/85 testing with voltage bias will fail these units. (for the unfamiliar, that's 85C 85%RH, 85hrs). Applying the bias may be a bit problematic with unpopulated boards, but I'm sure you can come up with something reasonable.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Reid
Sent: Friday, December 13, 2013 12:49 PM
To: [log in to unmask]
Subject: [TN] Crazing - the pictures
Hi Everyone,
I finally found Steve Gregory's email address. He has kindly posted some the pictures of the crazing that I found.
http://stevezeva.homestead.com/6494_2_1_mod.jpg
http://stevezeva.homestead.com/6494_M_001.jpg
http://stevezeva.homestead.com/6496_2_10.jpg
Sincerely,
Paul Reid
Program Coordinator
PWB Interconnect Solutions Inc.
235 Stafford Rd., West, Unit 103
Nepean, Ontario Canada, K2H 9C1
613 596 4244 ext. 229
Skype paul_reid_pwb
[log in to unmask]
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|