I agree with Russ' interpretation and that of the fabricator; that it is an externally observable condition.
However....
I started asking around a couple years ago (because of a failure we had in an NPTH) and found that no-one ever looks in NPTH's, ever. In my case the NPTH was pretty badly delaminated (not visible externally). The fab that built the board cross sectioned that hole and couldn't believe how bad it looked. But there's no criteria. (also by that point we had installed terminals so the roughness could have been caused by us.)
Here is a thought for the committee - should there be a criteria for evaluating NPTH's. (my apologies to all the fabricators that read this). I can imagine that NPTH drill bits do not receive the same level of scrutiny that a PTH bit does. Thoughts?
Pete
-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of Paul Reid
Sent: Thursday, December 05, 2013 4:06 PM
To: [log in to unmask]
Subject: [IPC-600-6012] Crazing
I was just on a conference call where we found crazing (a separation between glass fibers and the epoxy system), in a microsection. The fabricator stated that this had to be evaluated looking at a board macroscopically and could not be evaluated microscopically.
Crazing is called out in IPC-A- 600 in section 2, paragraph 2.3.2 page 18, which is "Externally Observable Characteristics". In A-600 there is picture of a microsection showing the defect but it states that a microsection is not required.
In IPC 6012-2010 crazing is call out in 3.3.2.2, page 12, which states (I am paraphrasing), "Crazing shall not violate greater than 50% of the distance between adjacent conductors..." The document then refers to IPC A 600.
What is your take on their argument that crazing should not be evaluated microscopically as per IPC?
Sincerely,
Paul Reid
Program Coordinator
PWB Interconnect Solutions Inc.
235 Stafford Rd., West, Unit 103
Nepean, Ontario Canada, K2H 9C1
613 596 4244 ext. 229
Skype paul_reid_pwb
[log in to unmask]
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|