TECHNET Archives

December 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Leland Woodall <[log in to unmask]>
Date:
Tue, 10 Dec 2013 11:11:29 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Reid <[log in to unmask]>
Message-ID:
Subject:
From:
Paul Reid <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (92 lines)
Hi Leland,

There are no laminate defects visible from a macroscopic evaluation. The
crazing is seen by microsection evaluation only.

Sincerely,  

 

Paul Reid 

Program Coordinator  

PWB Interconnect Solutions Inc. 
235 Stafford Rd., West, Unit 103 
Nepean, Ontario Canada, K2H 9C1 

613 596 4244 ext. 229  

Skype paul_reid_pwb 
[log in to unmask] 

 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: December 10, 2013 10:38 AM
To: [log in to unmask]
Subject: Re: [TN] Crazing

Victor,

I know we've been talking about crazing, but are you seeing any
blistering or delamination on these boards as well?

Leland

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Tuesday, December 10, 2013 10:14 AM
To: [log in to unmask]
Subject: Re: [TN] Crazing

   I just started to notice more and more laminate crazing around PTHs
barrels walls on LF solder and hybrid laminates.   IMHO it is a concern
that needs to be address.
Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete
Sent: Tuesday, December 10, 2013 8:42 AM
To: [log in to unmask]
Subject: Re: [TN] Crazing

Back to the microsection validity question - are you sure they aren't
trying to say that your microsectioning process caused the crazing, not
that it isn't a correct inspection method?

Pete

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

________________________________

"Confidentiality Notice:
This transmission (including any attachments) may contain confidential
information belonging to the sender and is intended only for the use of
the party or entity to which it is addressed. If you are not the
intended recipient, you are hereby notified that any disclosure,
copying, distribution, retention or the taking of action in reliance on
the contents of this transmission is strictly prohibited. If you have
received this transmission in error, please immediately notify the
sender and erase all information and attachments."

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2