Hi Vlad - just so we are all using terms on the same page, per the IPC
JSTD-002 committee: (1) Solderability is the ability of a surface(s) to
be wet molten solder and is a characteristic of the surface; (2)
Soldering-ability is the ability to make a solder connection as a function
of the process parameters. George and Joyce gave good working examples: if
I can take the QFN off the board and it passes the JSTD-002 testing, then
you have good solderability but bad soldering-ability.
Dave
From: "Vladimir Igoshev. PhD" <[log in to unmask]>
To: <[log in to unmask]>
Date: 12/26/2013 12:19 PM
Subject: Re: [TN] IPC-A-610E, Voids in Thermal exposed pad of QFNs
Sent by: TechNet <[log in to unmask]>
Well, in essence a solderability issue as it's about the ability of a
given QFN to be soldered and that ability will depend on the design,
the process etc. In many cases with various components a component
would easily pass the solderability test but fail to be soldered!
And it we won't call those defects 'voiding" then may be everyone will
realize that it's a different type of defect and won't rely on X-ray
trying to capture it.
--
Best regards,
Vladimir Igoshev. PhD
mailto:[log in to unmask]
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|