TECHNET Archives

November 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Neifer, Gebhard" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Neifer, Gebhard
Date:
Thu, 14 Nov 2013 08:47:22 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (43 lines)
Rich,
as far as I know UV-Ozone is not capable to remove inorganic contaminations. Plasma on the other hand can remove both, organic and inorganic residues...

Gebhard


-----Ursprüngliche Nachricht-----
Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Richard Kraszewski
Gesendet: Mittwoch, 13. November 2013 18:08
An: [log in to unmask]
Betreff: [TN] UV-Ozone Cleaning Processes

Are any of you familiar with UV-Ozone cleaning processes?  I am considering using Plasma to clean some PCA's prior to coating to improve wetting of coatings, but now wonder if I should also consider UV-Ozone.



Anyone care to state some pros and cons of each for my application?



Suprisingly enough, I don't see any mention of UV-Ozone cleaning in the IPC -CH65B handbook.



Thanks

Rich Kraszewski / Plexus





______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

**************************************************************************************** Note: If the reader of this message is not the intended recipient, or an employee or agent responsible for delivering this message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by replying to the message and deleting it from your computer. Thank you. ****************************************************************************************

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2